Polishing procedure and surface characterization lead tungstate crystal scintillator Road No. 723 and No. 754 [electronic resource].
- Published
- Washington, D.C. : United States. Dept. of Energy, 1996.
Oak Ridge, Tenn. : Distributed by the Office of Scientific and Technical Information, U.S. Dept. of Energy. - Physical Description
- 140 pages : digital, PDF file
- Additional Creators
- Lawrence Livermore National Laboratory, United States. Department of Energy, and United States. Department of Energy. Office of Scientific and Technical Information
Access Online
- Restrictions on Access
- Free-to-read Unrestricted online access
- Summary
- Step by step procedures are given for polishing the scintillator rods. A Strasbaugh spindle polishing machine was used along with visual inspection and hand polishing. Extensive data is given on pre-polish surface characterization, profilometry, microphotography, and interferometry.
- Report Numbers
- E 1.99:ucrl-id--124075
ucrl-id--124075 - Subject(s)
- Other Subject(s)
- Note
- Published through SciTech Connect.
05/01/1996.
"ucrl-id--124075"