Actions for Button
Button/Plate Yielding [electronic resource].
- Published
- Washington, D.C. : United States. Dept. of Energy. Office of Science, 1987.
Oak Ridge, Tenn. : Distributed by the Office of Scientific and Technical Information, U.S. Dept. of Energy. - Physical Description
- 2 pages : digital, PDF file
- Additional Creators
- Fermi National Accelerator Laboratory, United States. Department of Energy. Office of Science, and United States. Department of Energy. Office of Scientific and Technical Information
Access Online
- Restrictions on Access
- Free-to-read Unrestricted online access
- Summary
- An aluminum button and plate were yielded to compare the experimental and calculated button to plate stress ratios. Using the fact that compressive stress is directly proportional to area and load, the calculated button to plate stress ratio is equal to the plate to button area ratio for a constant load. The loads that caused the button and plate to yield were estimated from a load test cell graph obtained from the materials testing facility. The button was simply compressed, but the plate was compressed with a steel cylinder of the same diameter as the aluminum button. The experimental and calculated stress ratios for the button and plate are the same within experimental error. The equation for the plate bearing area is therefore correct.
- Report Numbers
- E 1.99:fermilab-d0-en-096
fermilab-d0-en-096 - Subject(s)
- Other Subject(s)
- Note
- Published through SciTech Connect.
06/17/1987.
"fermilab-d0-en-096"
Wintercorn, S. - Funding Information
- AC02-07CH11359